Just curious.... does anyone use Icebox rivets any more? Seems like an interesting idea when having to drive a large rivet.
MS20470D - Aluminum alloy, 2017-T or DD - Aluminum alloy, 2024-T composition don't seem very common. Interesting process to cook the rivet to 935º then quench it in water, then have about 15-20 minutes to work the rivet or refrigerate it to keep them soft for up to 2 weeks or so for later work.
There were a few threads on Van's Airforce about home builder using icebox rivets given they are so much easier to buck.
MS20470D - Aluminum alloy, 2017-T or DD - Aluminum alloy, 2024-T composition don't seem very common. Interesting process to cook the rivet to 935º then quench it in water, then have about 15-20 minutes to work the rivet or refrigerate it to keep them soft for up to 2 weeks or so for later work.
There were a few threads on Van's Airforce about home builder using icebox rivets given they are so much easier to buck.